how to resolve the sink marks issues by design scheme.

how to resolve the sink marks issues 

sink mark evaluation standard                           the guidelines for improve the sink                                                                                     mark by decrease plastic 

∅E ≤ 1.18A                                                                                                  ∅E ≤ 1.18A ,         D>10C







Example :

The maximum thickness in the red area is 2.55mm, which is more than 1.18 times the average wall thickness, so sink marks may occur in the red area.


decrease plastic  on the red surfaces.


this tthicken analysis result that it is decreased plastics below,  the maximum thickness from 2.55mm to1.70mm, so the sink marks can be avoided on the product surface.


#sink #mark #injection #molding #defect, #plastic #part #cosmetic #defect, #design #plastic #product #standard
话题标签

Best regards,
Maggie

ShenZhen HuaKaiYu Technology Co, Ltd. 

Mobile / Whatsapp/ Wechat /Teams :0086 15920030230
E-mail: sales@hky-technik.com 

Comments

Popular posts from this blog

16-cavity mold moulding, 96 lifters and 16 self-rotating inserts,

3DCS Variation Analyst for Yield Improvement

Powder Injection Molding Process